top of page


JEOL NeoScope JCM-5000 Benchtop Scanning Electron Microscope (SEM) (ICTAS I/Kelly Hal 420)
Facilities - Surface Analysis and Microscopy Equipment
-
Oriel 1000 W xenon arc lamp with an Ocean Optics S2000 bench-top spectrometer, including a linear CCD-array silicon detector responsive from 200 to 1100 nm
-
(2) Programmable Blue M ETC-04D-C with cascading compressors (-73˚C to 190˚C temperature range) interior dimensions: (610 x 457 x 457mm)
-
Programmable Espec SH-221 (-70˚C to 180˚C & 10% to 95% RH) interior dimensions: 30x25x30 cm
-
Programmable Espec ESX-4CA hygro-thermal cycling chamber (-70˚C to 150˚C & 10 to 98% RH) interior dimensions: 100 x 90 x 100 cm
-
(10) temperature/chemistry controlled submersion tanks with reflux system
-
1m3 Burn chamber with controlled heat flux exposure system